Alloy 46
Features:
Nickel Iron Alloy 46 /Glass Sealing 46 Alloy
Nominal composition,%
|
Alloy designation |
Ni |
Cr |
Mn |
Si |
C |
Al |
Fe |
P |
S |
|
Alloy 46 |
46.0 |
0.25 max |
0.80 max |
0.30 max |
0.05 max |
0.10 max |
Bal |
0.025 max |
0.025 max |